Janka hardness test

Janka hardness test

Test to measure resistance of wood


The Janka hardness test (English: /ˈæŋkə/;[1] German: [ˈjaŋka]), created by Austrian-born American researcher Gabriel Janka (1864–1932), measures the resistance of a sample of wood to denting and wear[citation needed] It measures the force required to embed an 11.28-millimeter-diameter (716 in) steel ball halfway into a sample of wood. (The diameter was chosen to produce a circle with an area of 100 square millimeters, or one square centimeter.)[2]

A common use of Janka hardness ratings is to determine whether a species is suitable for use as flooring. For hardwood flooring, the test usually requires an 80 mm × 150 mm (3 in × 6 in) sample with a thickness of at least 6–8 mm, and the most commonly used test is the ASTM D1037. When testing wood in lumber form, the Janka test is always carried out on wood from the tree trunk (known as the heartwood), and the standard sample (according to ASTM D143) is at 12% moisture content and clear of knots.[3]

The hardness of wood varies with the direction of the wood grain. Testing on the surface of a plank, perpendicular to the grain, is said to be of "side hardness". Testing the cut surface of a stump is called a test of "end hardness".[citation needed] Side hardness may be further divided into "radial hardness" and "tangential hardness", although the differences are minor and often neglected.

The results are stated in various ways, leading to confusion, especially when the actual units employed are often not attached. The resulting measure is always one of force. In the United States, the measurement is in pounds-force (lbf). In Sweden, it is in kilograms-force (kgf), and in Australia, either in newtons (N) or kilonewtons (kN). This confusion is greatest when the results are treated as units, for example "660 Janka".[4]

The Janka hardness test results tabulated below followed ASTM D 1037-12 testing methods. Lumber stocks tested range from 1" to 2" (25-50 mm) thick. The tabulated Janka hardness numbers are an average. There is a standard deviation associated with each species, but these values are not given.[citation needed] No testing was done on actual flooring.

Other factors affect how flooring performs: the type of core for engineered floorings, such as pine, HDF, poplar, oak, or birch; grain direction and thickness; floor or top wear surface, etc. The chart is not to be considered an absolute; it is meant to help people understand which woods are harder than others.

Typical Janka hardness values

More information Key ...
More information Species, Force: pounds-force (newtons) ...

References

  1. Baldwin, Elizabeth (5 January 2018). "The Scoop on Wood Hardness, Part 1: What is Janka?". hardwoodfloorsmag.com. National Wood Flooring Association. Retrieved 17 April 2021..
  2. "Janka hardness". Sizes.com. Retrieved 4 May 2021.
  3. "What is the Janka Hardness Scale". Avant Garde Flooring. 10 March 2019. Archived from the original on 15 July 2019. Retrieved 12 September 2019.
  4. Pedersen, Jason. "The Janka Hardness Test". Low Cost Flooring. Archived from the original on 15 March 2016. Retrieved 18 March 2016.
  5. Morlan, Johnny W. "Wood Species Janka Hardness Scale/Chart By Common/Trade Name A–J". The World's Top 125 Known Softest/Hardest Woods. Morlan wood gifts. Archived from the original on 26 April 2012. Retrieved 20 December 2011.
  6. "Quebracho". Lumber identification. The Wood Database. Archived from the original on 2016-03-04. Retrieved 2014-05-22.
  7. "Kingwood". Lumber identification. The Wood Database.
  8. "Cumaru". Lumber identification. The Wood Database.
  9. "Olive". The Wood Database. Archived from the original on 5 June 2023. Retrieved 15 December 2023.
  10. "Osage orange". Lumber identification. The Wood Database.[permanent dead link]
  11. "Olive". The Wood Database. Archived from the original on 3 June 2023. Retrieved 15 December 2023.
  12. "European Yew". The Wood Database. Archived from the original on 8 June 2023. Retrieved 15 December 2023.
  13. "English Oak". The Wood Database. Archived from the original on 3 March 2016. Retrieved 28 August 2015.
  14. "Wood charts", Custom workshop, archived from the original on 2013-01-06, retrieved 2018-11-30.
  15. "Radiata Pine". Lumber identification. The Wood Database. Archived from the original on 2016-08-11. Retrieved 2015-04-04.
  16. "Silver Maple". Lumber identification. The Wood Database. Archived from the original on 2016-08-09. Retrieved 2012-02-19.
  17. Wiepking, C. A.; Doyle, D. V. (November 1955). "Strength and related properties of Balsa and Quipo woods". UISDA Forest Service, Forest Products Laboratory: 27–28. Report No. 1511. {{cite journal}}: Cite journal requires |journal= (help) The record softness of 22 lbf is often falsely ascribed to quipo, but all such reports appear to be a misreading of figures 15 and 16 from this primary source, which makes clear that measurement is of balsa, and the softest quipo measured was 46 lbf tangential, 38 lbf radial.

Share this article:

This article uses material from the Wikipedia article Janka_hardness_test, and is written by contributors. Text is available under a CC BY-SA 4.0 International License; additional terms may apply. Images, videos and audio are available under their respective licenses.